Direct leaching of manganese from pyrolusite using low-grade manganese carbonate as a reducing agent in dilute sulphuric acid was investigated by blending pyrolusite with manganese carbonate ore, which has the reductant ferrous carbonate. The effects of leaching temperature, sulphuric acid concentration, leaching time, stirring speed, particle size etc. were considered. The results generally show that as the various parameters increase, the recovery of Mn increases while Fe decreases. A blend ratio of 5 : 1 by weight of manganese carbonate-pyrolusite gave 96% maximum extraction of manganese by the following conditions: leaching time of 120 min, leaching temperature of 70°C, stirring speed of 300 r/min, particles size of+150 mesh, liquid-solid ratio of 14 : 1 and acid concentration of 200 g/L. The leaching process followed a first-order reaction and the rate constant with respect to manganese was found to be 0.33 h~(-1) with activation energy of 9.5 kJ/mol.
机译:通过将软锰矿与具有还原性碳酸亚铁的碳酸锰矿石混合,研究了使用低级碳酸锰作为还原剂在稀硫酸中从软锰矿中直接浸出锰。考虑浸出温度,硫酸浓度,浸出时间,搅拌速度,粒径等的影响。结果通常表明,随着各种参数的增加,Mn的回收率增加而Fe的回收率降低。碳酸锰-软锰矿的重量比为5:1,在以下条件下锰的最大萃取量为96%:浸出时间120分钟,浸出温度70°C,搅拌速度300 r / min,粒径+150目,液固比14:1,酸浓度200 g / L。浸出过程遵循一级反应,相对于锰的速率常数为0.33 h〜(-1),活化能为9.5 kJ / mol。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号