This paper describes a novel hydrothermal method for preparing potassium sulfate and zeolite NaA from K-feldspar ore. The 3-step process involves the hydrothermal decomposition of K-feldspar, the preparation of potassium sulfate from kalsilite, and the synthesis of zeolite NaA from alumina-silica residue. K-feldspar transformed into kalsilite in a KOH solution at 280 degrees C. K2O was extracted from kalsilite at a rate of 95.73% by using H2SO4 (5.5 wt.%) and kalsilite at a mass ratio of 6.26 and a temperature of 60 degrees C for 4 h. Subsequently, agricultural grade potassium sulfate was crystallized by direct evaporation of the resulting K2SO4 solution. The CEC value of zeolite NaA produced from the alumina-silica residue was 168 mg CaO/g, making it a suitable substitute for conventional phosphatic washing builders. The method is a simple, clean and energy-efficient method for the utilization of K-feldspar ores. (C) 2016 Elsevier B.V. All rights reserved.
机译:本文介绍了一种新型的水热法,用于从钾长石矿石中制备硫酸钾和NaA沸石。分三步进行的过程包括钾长石的水热分解,由钾铝石制备硫酸钾和由氧化铝-二氧化硅残余物合成沸石NaA。在280℃的KOH溶液中转化为钾长石的钾长石。通过使用H2SO4(5.5 wt。%)和质量比率为6.26的钾硅石,以95.73%的比率从钾硅石中提取K 2 O。持续4小时。随后,通过直接蒸发所得的K2SO4溶液使农业级硫酸钾结晶。由氧化铝-二氧化硅残余物生产的沸石NaA的CEC值为168 mg CaO / g,使其成为常规磷酸盐洗涤助洗剂的合适替代品。该方法是利用钾长石矿石的一种简单,清洁且节能的方法。 (C)2016 Elsevier B.V.保留所有权利。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号