The principal failure mechanism in thixoforming dies is expected to be thermal fatigue, as the mechanical loading on tooling is modest owing to a semisolid feedstock. High process temperatures during steel thixoforming induce high compressive strains at the die cavity surface during slurry injection. The magnitudes of the thermal gradient and strains that develop on the cavity surface are directly linked with the temperature of the die surface immediately before slurry injection. An increase in die bulk temperature from 450 to 550 deg C reduces the surface to interior temperature differential and thus the surface strains by as muph as 30 percent, a very favourable effect from thermal fatigue point of view.
机译:触变性成型模具的主要失效机理是热疲劳,因为半固体原料对模具的机械负荷不大。钢触变成形过程中的高工艺温度会在注浆过程中在模腔表面产生高压缩应变。刚好在注入浆液之前,腔体表面上产生的热梯度和应变的大小与模具表面的温度直接相关。模具体积温度从450摄氏度增加到550摄氏度,减小了表面到内部的温差,因此表面应变降低了30%,从热疲劳的角度来看,这是非常有利的效果。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号