Regressive orthogonal design experiments have been carried out based on the analysis of the oxidation and induration behaviours of individual magnetite and hematite pellets. The research shows that the optimal pellet preheating time and temperature, and roasting time and temperature change with hematite/magnetite (H/M) ratio. Under the conditions of preheating temperature 900 deg C, preheating time 10 min, roasting temperature 1275 deg C and roasting time 15 min, the compression strength of preheated and roasted pellets is found to be respectively more than 444 N/pellet (N/P) and 3993 N/P when the magnetite content in the pellets exceeds 20 percent. The pellet strengths meet the requirements of rotary kilns and blast furnaces respectively.
机译:基于对单个磁铁矿和赤铁矿球团的氧化和硬结行为的分析,进行了回归正交设计实验。研究表明,最佳的颗粒预热时间和温度,以及焙烧时间和温度随赤铁矿/磁铁矿(H / M)比的变化而变化。在预热温度为900℃,预热时间为10分钟,焙烧温度为1275℃,焙烧时间为15分钟的条件下,预热和焙烧的颗粒的抗压强度分别大于444 N /粒(N / P)。当粒料中磁铁矿含量超过20%时为3993 N / P。颗粒强度分别满足回转窑和高炉的要求。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号