【24h】

Damage evolution during creep of steels

机译:钢蠕变过程中的损伤演变

获取原文
获取原文并翻译 | 示例
           

摘要

Using high-precision constant-stress machines, normal creep curves are recorded over tensile stress ranges giving creep lives up to about 1000h or more for 0.5Cr-0.5Mo-0.25V ferritic steel, 1Cr-lMo-0.25V bainitic steel, 316L austenitic steel and the oxide-dispersion-strengthened 14% Cr ferritic steel, Incoloy MA957. Although the curve shapes are material and test condition sensitive, a minimum rate rather than a secondary or steady-state value always occurs when the decaying primary rate is offset by the tertiary acceleration. The observed behaviour patterns are analysed with special reference to the measured values of the creep damage tolerance parameter and microstructural evidence on the various damage processes governing tertiary creep and fracture.
机译:使用高精度恒应力机器,可在拉伸应力范围内记录正常的蠕变曲线,对于0.5Cr-0.5Mo-0.25V铁素体钢,1Cr-1Mo-0.25V贝氏体钢,316L奥氏体钢,蠕变寿命可达到约1000h或更长钢和氧化物弥散强化的14%Cr铁素体钢,Incoloy MA957。尽管曲线形状对材料和测试条件敏感,但是当衰减的一次速率被三次加速度抵消时,始终会出现最小速率而不是次要值或稳态值。分析观察到的行为模式,并特别参考蠕变损伤容限参数的测量值以及控制第三级蠕变和断裂的各种损伤过程的微观结构证据。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号