Copper catalysts supported on MFI-type metallosilicate were prepared and their activities for selective oxidation of NH_3 were examined. Among the catalysts tested in this study, copper catalysts supported on MFI-type metallosilicate showed the highest activity. This catalyst selectively converted NH_3 to N_2 at 250-400 deg C in the presence of excess oxygen. The characterization of acidity and the effect of copper content revealed that active site of the catalyst in selective oxidation of NH_3 was the copper supported on the strong acidic site of metallosilicate. From NH_3-TPD, NH_3-O_2 pulse reaction and FT-IR measurements, amino groups formed on the catalyst surface were found to be intermediates of the NH_3 selective oxidation. The following mechanism for the selective oxidation of NH_3 was suggested; NH_3 is first adsorbed on the Bronsted acid site of metallosilicate and then converted to NH_4~+. Secondly, dinitrogen group intermediate is formed by the oxidative dehydration of NH_4~+. Finally, dinitrogen group intermediate is dehydrated oxidatively to N_2.
机译:制备支持MFI型金属硅酸盐的铜催化剂,并检查它们的选择性氧化NH_3的活性。在本研究中测试的催化剂中,负载在MFI型金属硅酸盐上的铜催化剂显示出最高的活性。该催化剂在过量氧的存在下在250-400℃下选择性地转化为250-400℃的NO_2。酸度的表征和铜含量的作用显示,催化剂的活性位点在NH_3的选择性氧化中是铜酸硅酸盐的强酸位点。来自NH_3-TPD,NH_3-O_2脉冲反应和FT-IR测量,发现在催化剂表面上形成的氨基是NH_3选择性氧化的中间体。提出了以下对NH_3选择性氧化的机制;首先吸附在金属硅酸盐的正稳酸部位上的NH_3,然后转化为NH_4〜+。其次,通过NH_4〜+的氧化脱水形成了二氮基团中间体。最后,二氮基团中间体氧化于N_2。

著录项

  • 来源
  • 作者单位

    Hiroshima R &

    D Center Mitsubishi Heavy Industries LTD;

    4-6-22 Kanonshin-machi Nishi-ku Hiroshima-shi 733-8553 Japan and Power Systems Headquarters Mitsubishi Heavy Industries LTD;

    3-3-1 Minatomirai Nishi-ku Yokohama-shi 220-0012 Japan;

    Hiroshima R &

    D Center Mitsubishi Heavy Industries LTD;

    4-6-22 Kanonshin-machi Nishi-ku Hiroshima-shi 733-8553 Japan and Power Systems Headquarters Mitsubishi Heavy Industries LTD;

    3-3-1 Minatomirai Nishi-ku Yokohama-shi 220-0012 Japan;

    Hiroshima R &

    D Center Mitsubishi Heavy Industries LTD;

    4-6-22 Kanonshin-machi Nishi-ku Hiroshima-shi 733-8553 Japan and Power Systems Headquarters Mitsubishi Heavy Industries LTD;

    3-3-1 Minatomirai Nishi-ku Yokohama-shi 220-0012 Japan;

  • 收录信息
  • 原文格式 PDF
  • 正文语种 jpn
  • 中图分类 化学;化学工业;
  • 关键词

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号