Flexible thermoelectric generator with polydimethyl siloxane in thermoelectric material and substrate

机译:在热电材料和基材中具有聚二甲基硅氧烷的柔性热电发生器

获取原文
获取原文并翻译 | 示例
           

摘要

In this paper, the fabrication and characterization of a flexible thermoelectric generator (TEG) is presented. Bismuth telluride powder (Bi/Te) is utilized as p- and n-type thermoelectric materials, and carbon nanotubes (CNTs) are used to enhance electrical conductivity. Both the CNTs and bismuth telluride (Bi/Te) powder are mixed with a solution of polydimethyl siloxane (PDMS) as a precursor. The same PDMS used for the hybrid thermoelectric materials is also used as the substrate, making the TEG flexible and increasing its stability. The Seebeck coefficients of the fabricated p- and n-type thermoelectric materials are 143 and -174 mu V/K, respectively. The output voltage of the fabricated device is 920 mV and the generated power is 570 mu W/cm(2) with a temperature difference of 60 degrees C. The fabricated TEG maintains its performance level during bending reliability tests on a curvature with a radius as small as 5 mm, and after more than 1000 repetitions of bending on a curvature with a radius of 20 mm. (C) 2016 Published by Elsevier B.V.
机译:本文介绍了柔性热电发电机(TEG)的制造和特性。碲化铋粉末(Bi / Te)用作p型和n型热电材料,碳纳米管(CNTs)用于增强导电性。将CNT和碲化铋(Bi / Te)粉末都与作为前体的聚二甲基硅氧烷(PDMS)溶液混合。用于混合热电材料的相同PDMS也用作基材,从而使TEG具有柔性并增加了其稳定性。所制造的p型和n型热电材料的塞贝克系数分别为143和-174μV/ K。制成的设备的输出电压为920 mV,产生的功率为570μW / cm(2),温度差为60摄氏度。制成的TEG在弯曲可靠性测试期间保持其性能水平,其曲率半径为小到5毫米,并在半径20毫米的曲率上重复弯曲1000多次。 (C)2016由Elsevier B.V.发布

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号