The Effect of Jet Flow Impingement on the Corrosion Products Formed on a Pipeline Steel in Naturally Aerated Sour Brine

机译:喷射流冲击对天然气酸盐盐水管道钢上形成的腐蚀产物的影响

获取原文
获取原文并翻译 | 示例

摘要

Corrosion was generated by the action of a jet impingement flow of sour brine on pipeline steel samples of X70. Flow-assisted corrosion affected nature, number and peak intensity of the chemical species formed as corrosion products. Iron sulfides predominated in static and low flow rate conditions (1.1m/s), whereas at 2.4m/s iron oxides were mainly formed, which led to higher corrosion rates and suggested that oxides are less protective than sulfides. On inhibition, imidazoline seems to mitigate oxide formation and support sulfide formation balancing both species on steel surface. Ferrite phase in laminar pearlite was preferentially dissolved with/without inhibitor, and mackinawite (FeS2) was formed at every flow rate, angle with and without inhibitor. Theoretical stresses determined by computational flow dynamics for corrosion product removal showed a fair approximation to those proposed in the literature.
机译:通过酸盐的喷射冲击流动对X70的管道钢样品的作用产生腐蚀。 流动辅助的腐蚀影响了作为腐蚀产品形成的化学物种的性质,数量和峰值强度。 在静态和低流量条件下占主导的铁硫化物(1.1M / s),而主要形成2.4M / s的氧化铁,这导致腐蚀速度较高,并表明氧化物比硫化物更少保护。 在抑制作用上,咪唑啉似乎减轻了氧化物形成并支持硫化物形成平衡钢表面上的两个物种。 层状珠光体中的铁素体相优选溶解/不含抑制剂,并且在每个流速,与抑制剂的每个流速,角度形成鲭岩(FES2)。 通过计算流动动力学确定用于腐蚀产品的理论应力,对文献中提出的那些进行了公平的近似。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号