An environmentally friendly superhydrophobic modified polyurethane sponge by seashell for the efficient oil/water separation

机译:由贝壳的环保超疏水改性聚氨酯海绵用于高效的油/水分离

获取原文
获取原文并翻译 | 示例
           

摘要

Seeking eco-friendly, highly -efficient, low-cost, and robust adsorbents to remove oil from water resources are very much in demand. In this work, an environmentally friendly, recyclable, superhydrophobic, and superoleophilic seashell/epoxy resin/polyurethane (EP/SPU) sponge with contact angle of 174.10 ? 0.47 ? was prepared. EP/SPU sponge demonstrated high adsorption capacity in the range of 28.03-42.17 g/g times more than of its own weight for five oils and four organic solvents. The EP/SPU sponge was used 10 times for the adsorption of the oils and organic solvents with no significant loss in its adsorption capacity. The mechanical test suggested that the lightweight EP/SPU sponge is not compressible compared with neat polyurethane (PU) sponge. The volume of neat PU sponge decreased from 2.28 to 1.14 cm 3 while the EP/SPU sponge volume (2.28 cm 3 ) did not change. As a result, EP/SPU sponge is expected to be a promising sorbent for potential applications in the cleanup of oil spills from water.
机译:寻求环保,高效,低成本和稳健的吸附剂,以从水资源中除去油状况。在这项工作中,环保,可回收的,超疏水和高脂骨壳/环氧树脂/聚氨酯(EP / SPU)海绵,接触角为174.10? 0.47?准备好了。 EP / SPU海绵在五个油脂和四种有机溶剂的其重量的范围内显示出高吸附容量。使用EP / SPU海绵10次,用于吸附油和有机溶剂,其吸附能力没有显着损失。机械测试表明,与纯聚氨酯(PU)海绵相比,轻质EP / SPU海绵不可压缩。纯净的PU海绵的体积从2.28降至1.14厘米3,而EP / SPU海绵体积(2.28厘米3)没有变化。结果,预计EP / SPU海绵将成为潜在的应用在水中的潜在应用。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号