In the iron and steel industry, the production of narrow particle size distribution (PSD) for pellet feed making with acceptable liberation of valuables from the iron ore is very difficult. This study has been carried out to achieve desired pellet feed with narrow PSD and maximum liberation of hematite from the iron ore. The iron ores have been collected from three different sources (mines in Karnataka state) and milled. The iron ores and the blend feed samples were analyzed in the Optical Microscope (OM) and Quantitative Evaluation of Minerals by Scanning Electron Microscopy (QEMSCAN) to understand the PSD and percentage of hematite liberation. The new approach is adapted to identify the retention time (RT) of the iron ore in the mill, and the total RT taken for the blend sample in the Bond's ball mill is considered as the reference grinding time for milling in the Laboratory Ball Mill (LBM). The desired narrow PSD (- 150/+ 10 mu m) with acceptable hematite liberation is achieved at an optimal grinding time of 7 min in the LBM.
机译:在钢铁工业中,生产窄粒度分布(PSD)的颗粒饲料制作,可接受的铁矿石贵重物品的解放非常困难。已经进行了该研究,以实现具有窄PSD的所需颗粒饲料,并从铁矿石中最大限度地释放赤铁矿。铁矿石已从三种不同的来源(Karnataka状态的矿区)收集并研磨。在光学显微镜(OM)中分析铁矿石和混合物进料样品,并通过扫描电子显微镜(QEMSCAN)来定量评估矿物质,以了解赤铁矿释放的PSD和百分比。新方法适于鉴定磨机中铁矿石的保留时间(RT),并且在粘合的球磨机中的混合物样品所取的总体室被认为是在实验室球磨机中研磨的参考磨削时间( LBM)。具有可接受的赤铁矿释放的所需的窄PSD( - 150 / +10μm)在LBM中7分钟的最佳研磨时间实现。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号