Objectives: To examine the initial shear bond strength of orthodontic brackets bonded to bleached teeth with a self-etching adhesive system, as well as the effect of the length of time after bleaching on the initial bond strength. Method and Materials: Ninety premolars were collected and divided equally among a control group (CG) of unbleached teeth with brackets bonded, an immediate group (IG) with teeth bonded soon after bleaching, and a delayed group (DG) consisting of teeth bleached and then immersed in artificial saliva for 7 days before bracket bonding. Subsequently, the teeth of each group were equally assigned to two different primer adhesive systems: the acid-etch-and-rinse adhesive system (35% phosphoric acid gel and Transbond XT primer) and the self-etching adhesive system (Transbond Plus self-etching primer). Initial bond strength was measured 24 hours after bracket bonding. Results: IG registered the lowest mean initial bond strength when the self-etching adhesive system was in use, followed by DG and CG (in that order). As for the acid-etch-and-rinse adhesive system, the mean initial bond strength was significantly lower in IG than in CG and DG. Significant differences in mean initial bond strength were noted between the two adhesive systems in IG and DG. Conclusion: In trials using a self-etching adhesive system, the mean initial bond strength that declined immediately after bleaching returned to a clinically acceptable level of 6 MPa after the specimens were immersed in artificial saliva for 7 days but fell short of the level of unbleached teeth. (Quintessence Int 2012;43:e60?e66).
机译:目的:用自蚀刻粘合剂系统检查粘合漂白牙齿的初始剪切粘合强度,以及在初始粘合强度漂白后的时间长度的效果。方法和材料:收集九十珠粒并在漂白括号中的括号(Ig)粘合的括号中的对照组(Cg)中分开,并且在漂白后很快键合,延迟组(DG)和由牙齿漂白的延迟组(DG)组成然后浸入人造唾液中,在支架粘合前7天。随后,将每组的牙齿同等地分配到两个不同的底漆粘合剂系统:酸蚀刻和冲洗粘合剂系统(35%磷酸凝胶和替螺纹XT底漆)和自蚀刻粘合剂系统(横桥加自我 - 蚀刻底漆)。在支架粘合后24小时测量初始粘合强度。结果:Ig在使用自蚀刻粘合剂系统时,注册了最低的平均键合强度,然后是DG和CG(按此顺序)。至于酸蚀刻和冲洗粘合剂系统,IG的平均初始粘合强度明显低于CG和DG。在IG和DG的两个粘合剂系统之间注意到平均初始粘合强度的显着差异。结论:在使用自蚀刻粘合剂体系的试验中,在将样品浸入人工唾液中浸渍后,在漂白后返回临床可接受水平的平均初始粘合强度返回到临床上可接受的6MPa后7天,但缩短了未漂白的水平。牙齿。 (Quintessence int 2012; 43:E60?E66)。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号