The remelting behavior of the hot-work tool steel X37CrMoV5-1 is investigated with several experimental melts on a lab-scale ESR-plant. The investigated parameters comprise a variation of the slag compositions and the use of a protective nitrogen atmosphere. Variations of the slag composition include slags with different contents of CaF2, CaO, and Al2O3 as well as a variation of the SiO2-content in the slag. The remelted ingots are forged and analyzed regarding their chemical composition. The distribution and composition of the non-metallic inclusions (NMI) is studied by an automated SEM-EDX method. Additionally, the chemical composition of the slag after remelting is analyzed. The results show clearly an equilibrium reaction between Si and Al in the steel with SiO2 and Al2O3 in the slag as well as the effect of oxygen in open ESR operation. A protective atmosphere reduces the Si-losses during remelting, but has no major effect on the number or composition of NMI compared to open remelting. The content of NMI, especially the larger ones, is reduced significantly in all remelting experiments. The majority of the NMI are MA-spinel type except for the CaO-free slag, where alumina inclusions prevail. In general, remelting leads to an almost complete removal of sulfides, a reduction of oxisulfides, and a slight increase of oxides.
机译:研究了热加工工具钢X37Crmov5-1的重熔行为,在实验室级ESR植物上进行了几种实验熔体。研究的参数包括炉渣组合物的变化和使用保护氮气氛。炉渣组合物的变化包括具有CAF2,CaO和Al 2 O 3的不同含量的炉渣以及炉渣中的SiO 2含量的变化。对其化学组成的伪造锭进行了锻造和分析。通过自动化的SEM-EDX方法研究非金属夹杂物(NMI)的分布和组成。另外,分析了重熔后炉渣的化学成分。结果表明,在炉渣中,钢中的Si和Al与Al2O3之间的平衡反应以及氧气在开放ESR操作中的作用。保护气氛在重熔过程中降低了Si导损,但与开口重熔相比,对NMI的数量或组成没有重大影响。在所有重熔试验中,NMI,尤其是较大的含量显着减少。大多数NMI是MA-Spinel类型,除了无甲渣,其中氧化铝夹杂物占上风。通常,重熔导致几乎完全除去硫化物,降低氧化硫化物,略微增加。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号