Analysis of Key Factors Affecting the Lifetime of Blue Phosphorescent OLED Using CN Modified Blue Host Materials

机译:用CN改性蓝色主体材料分析影响蓝磷光OLED寿命的关键因素

获取原文
获取原文并翻译 | 示例

摘要

Three host materials were synthesized for blue phosphorescent organic light emitting diodes (OLEDs) by combining carbazolylcarbazole and benzonitrile. Each material has different CN positions relative to the carbazolylcarbazole donor as ortho,-meta, and para. These materials were used for finding fundamental factors of lifetime degradation of blue OLEDs. By comparing the characteristics of the three hosts with the CN unit at ortho, meta and para positions, we studied the effects of the CN position on the lifetime of the blue phosphorescent OLEDs. We calculated bond dissociation energy of the three hosts and energy transfer to find key factors about degradation. We calculated Forster energy transfer rate from host to dopant by measuring parameters for the calculation. The correlation of the device lifetime with the parameters revealed that the bond dissociation energy and Forster energy transfer rate are critical to the device lifetime of the blue phosphorescent OLEDs.
机译:通过组合咔唑基咔唑和苯腈来合成三个主体材料,用于蓝磷光有机发光二极管(OLED)。 各种材料相对于咔唑基咔唑供体具有不同的CN位置,如邻奥醇, - 粒子和律。 这些材料用于寻找蓝橄榄寿命劣化的基本因素。 通过将三个宿主的特性与CN单元进行比较,在Ortho,Meta和Para位置,我们研究了CN位置对蓝磷光OLED的寿命的影响。 我们计算了三个主机和能量转移的债券解离能,以找到有关降解的关键因素。 通过测量计算参数,从宿主计算到掺杂剂的Forster能量转移率。 器件寿命与参数的相关性显示,粘合解离能和福尔斯特能量转移率对蓝磷光OLED的器件寿命至关重要。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号