The powder metallurgy high-strength Ti-1Al-8V-5Fe alloy (Ti-185 alloy) was investigated in this paper with different addition methods of alloying elements, Al, V, Fe pure elements powder (EP) or 1Al-8V-5Fe ternary master alloy powder (MAP), based on TiH2 powders at the sintering temperature from 1150 to 1350 degrees C. The results indicate that the Ti-185 alloy with the 1Al-8V-5Fe master alloy (Ti-185 MAP alloy) possesses the higher relative sintered density, less oxygen content, and less -phase volume fraction versus the Ti-185 alloy with Al, V, and Fe pure elements (Ti-185 EP alloy). No matter where the sintering temperature is 1150, 1250, or 1350 degrees C, Ti-185 MAP alloy invariably has the higher yield strength and hardness which have a strong relationship to its higher density and less volume fraction of softer -phase in comparison with Ti-185 EP alloy.
机译:本文研究了粉末冶金高强度Ti-1AL-8V-5FE合金(TI-185合金),采用合金元素,Al,V,Fe纯元粉(EP)或1AL-8V-5FE不同的添加方法 基于TiH2粉末的三元母合金粉末(MAP)从1150至1350℃的烧结温度。结果表明,Ti-185合金与1AL-8V-5FE主合金(TI-185地图合金)具有 具有较高的相对烧结密度,较少的氧含量和低于相对的体积级分,与TI-185合金与Al,V和Fe纯元素(Ti-185 EP合金)相比。 无论烧结温度为1150,1250,或1350℃,TI-185地图合金是否具有更高的屈服强度和硬度,与其较高的密度和更少的较低的柔软体积分数相比具有较强的关系。与TI相比 -185 ep合金。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号