> In this study, the tribological performance of polyamide‐6 (PA‐6), polypropylene (PP), polyamide‐6/polypropylene (PA‐6/PP) polymer blend, and nanoclay reinforced polyamide‐6/polypropylene composite are investigated. Nanoclay reinforced polymer composite is produced by melt compounding using co‐rotating twin screw extruder followed by injection moulding. Tribological studies are carried out using a pin‐on‐stainless steel disc configuration under dry sliding conditions. Tribological tests are carried out at sliding speed of 0.5?m?s ?1 and applied load values of 25, 50,100, 150?N. The friction coefficient and specific wear rate values are obtained and evaluated. The results show that the addition of nanoclay into the PA‐6/PP polymer blend reduced their coefficient of friction and specific wear rate values. The lowest coefficient of friction and specific wear rate values are for nanoclay reinforced PA‐6/PP blend. The highest coefficient of friction and specific wear rate values are for PA‐6 polymer.
机译: <第XML:ID =“Masy201700022-SEC-0001”>

在本研究中,多酰胺-6(PA-6),聚丙烯的摩擦学性能。 (PP),聚酰胺-6 /聚丙烯(PA-6 / PP)聚合物共混物和纳米粘土增强聚酰胺-6 /聚丙烯复合材料进行了研究。通过使用共旋转双螺杆挤出机进行熔融配合,然后采用注射成型,通过熔融配合制备纳米铬增强聚合物复合材料。在干式滑动条件下使用销不锈钢盘配置进行摩擦学研究。摩擦学检测在0.5Ω·s α1的滑动速度下进行,并且施加的载荷值为25,50,100,150≤n。获得并评估摩擦系数和特定的磨损率值。结果表明,将纳米粘土加入PA-6 / PP聚合物共混物降低了它们的摩擦系数和特定的磨损率值。最低系数的摩擦系数和特定磨损率值对于纳米粘土增强PA-6 / PP混合物。最高摩擦系数和特定磨损率值适用于PA-6聚合物。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号