This paper explored a solid-phase reduction method to prepare ultrafine nickel powder under different conditions. The effect of a NaCl separator agent on the morphology, primary particle size and specific surface area of the prepared nickel powder is discussed. The results show that direct contact among primary Ni particles can be effectively inhibited during the reduction of nickel oxalate due to the presence of the NaCl separator agent. An ultrafine nickel powder with a primary particle size of between 80 and 150 nm can be prepared with NaCl as the separator agent at temperatures from 400 degrees C to 460 degrees C. The powder reduced at 430 degrees C has a uniform particle distribution and a decreased amount of agglomeration. (c) 2020 Published by Elsevier B.V. on behalf of The Society of Powder Technology Japan. All rights reserved.
机译:本文探讨了在不同条件下制备超细镍粉的固相减少方法。 讨论了NaCl分离剂对制备的镍粉的形态,一次粒度和比表面积的影响。 结果表明,由于NaCl分离剂的存在,可以有效地抑制原发性Ni颗粒之间的直接接触。 具有初级粒径为80和150nm的超细镍粉,可以用NaCl作为分离剂在400℃至460℃的温度下制备。在430℃下降低粉末具有均匀的颗粒分布和减少 聚集量。 (c)2020年由elsevier b.v发表的。代表日本粉末科技会。 版权所有。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号