Influence of fly ash and steam on microstructure, and mechanical properties of oxide bonded porous SiC ceramics

机译:粉煤灰和蒸汽对微观结构的影响,氧化物粘结多孔SiC陶瓷的力学性能

获取原文
获取原文并翻译 | 示例
       

摘要

Ceramic filters specially SiC filters are used in advanced coal combustion and gasification processes to remove fine dust particles from the fuel gas at high temperatures and high pressure for protection of turbine blades and other downstream components from corrosion and erosion and to meet the environmental regulations. Processing of corrosion resistant porous SiC ceramics at low temperature using a simple technique is still challenging. In this study oxide bonded porous SiC ceramics were synthesized by cost effective method. The corrosion behaviour of SiC ceramic filter materials in presence of steam, coal ash and both coal ash and steam was investigated at 1000 degrees C for 96-240 h. The apparent changes in mass, porosity and density with corrosion duration and environment were recorded. Finally SEM, XRD and mechanical tests of the corroded samples were carried out. The corrosion test results indicated water vapour is the perpetrator for strength degradation. (C) 2019 SECV. Published by Elsevier Espana, S.L.U.
机译:陶瓷过滤器专门的SiC过滤器用于高级煤燃烧和气化过程中,以在高温下从燃料气体中除去细小的粉尘颗粒,以及保护涡轮机叶片和其他下游部件免受腐蚀和侵蚀的影响,并满足环境法规。使用简单的技术在低温下加工耐腐蚀多孔SiC陶瓷仍然具有挑战性。在该研究中,通过成本有效的方法合成了氧化物键合多孔SiC陶瓷。在1000℃下,在1000℃下对蒸汽,粉煤灰和煤灰和蒸汽存在的SiC陶瓷过滤材料的腐蚀行为在96-240小时。记录了腐蚀持续时间和环境的质量,孔隙度和密度的表观变化。最后进行SEM,XRD和腐蚀样品的机械测试。腐蚀试验结果表示水蒸气是强度降解的肇率。 (c)2019 SECV。 elsevier espana发布,s.l.u。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号