This paper compares the remineralization of human natural caries and artificial caries-like dentin lesions treated with a novel whisker-reinforced experimental composite resin (ART composite) with a resin-modified glass ionomer cement (RM-GIC) as control. Ten molars with moderate natural dentin caries were prepared (N). Artificial caries-like dentin lesions were prepared in occlusal dentin of 10 caries-free molars and demineralized at pH 4.3 for 48 h (A). The cavities were restored with ART composite or RM-GIC. All restored teeth were sliced into 120 mum sections. Transverse microradiography combined with digital image analysis was performed to analyze the change in mineral density at the same position in the specimens before and after 4 and 8 weeks remineralization/demineralization treatment. The mean percent remineralization +/- standard deviation after 4 and 8 weeks are: N with ART composite, 27 +/- 9 and 46 +/- 14, respectively; N with RM-GIC, 18 +/- 6 and 36 +/- 11, respectively; A with ART composite, 48 +/- 9 and 66 +/- 11, respectively; A with RM-GIC, 50 +/- 13 and 62 +/- 11, respectively. There was a significant difference between the ART composite and RM-GIC for the remineralization of natural caries (P<0.05). For both restoratives there were significant differences between the remineralization of natural and artificial caries (P<0.001). The ART composite and RM-GIC remineralized natural and artificial caries differently, most likely due to differences in the microstructure and composition of the caries dentin.
机译:本文比较了一种新型晶须增强的实验复合树脂(ART复合材料)与树脂改性的玻璃离聚物水泥(RM-GIC)作为对照治疗的人类天然龋齿和人造龋齿样牙本质病变的再矿化作用。制备十颗具有中等天然牙本质龋齿的臼齿(N)。在10个无龋齿的咬合牙本质中制备人造龋齿样牙本质病变,并在pH 4.3下脱矿质48小时(A)。用ART复合材料或RM-GIC修复空腔。将所有修复的牙齿切成120毫米的切片。进行横向显微放射照相与数字图像分析相结合,以分析再矿化/去矿化处理4周和8周之前和之后样品中相同位置的矿物质密度的变化。 4和8周后的平均再矿化百分比+/-标准偏差为:N与ART复合材料分别为27 +/- 9和46 +/- 14。 N与RM-GIC分别为18 +/- 6和36 +/- 11;具有ART复合材料的A,分别为48 +/- 9和66 +/- 11;带有RM-GIC的A,分别为50 +/- 13和62 +/- 11。 ART复合材料与RM-GIC在天然龋齿的再矿化方面存在显着差异(P <0.05)。对于这两种修复剂,天然和人工龋齿的再矿化之间存在显着差异(P <0.001)。 ART复合材料和RM-GIC对天然和人工龋齿的矿化程度不同,这很可能是由于龋齿的微观结构和成分不同所致。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号