Mesoporous amorphous TiO2 shell-coated ZIF-8 as an efficient and recyclable catalyst for transesterification to synthesize diphenyl carbonate

机译:中孔无定形TiO2壳涂覆的ZIF-8作为用于酯交换的有效和可回收的催化剂,以合成二苯基碳酸酯

获取原文
获取原文并翻译 | 示例
           

摘要

The catalysts containing tetra-coordinated titanium have been widely used for transesterification. The key issue in the design of these catalysts is the stability of tetra-coordinated titanium. In this study, mesoporous amorphous titanium oxides coated on a zeolitic imidazolate framework (ZIF-8) were developed by using a hexadecylamine (HDA) surfactant as a structure-directing agent. The mesopores surface areas of the amorphous TiO2 shell could be simply controlled by changing the dosage of HDA in the synthetic process. The novel, efficient and recyclable heterogeneous catalyst was introduced to the synthesis of diphenyl carbonate from dimethyl carbonate and phenyl acetate for the first time. The catalyst structure was characterized by X-ray diffraction, scanning electron microscopy, transmission electron microscopy, nitrogen adsorption-desorption, Fourier transform infrared spectroscopy and thermogravimetric analysis. The effects of the molar ratio of Ti to Zn, HDA amount, catalyst amount, reaction time and reusability on the yield of the transesterification products were also determined. The results showed that the mesopores of TiO2 shell facilitated reactants and productions diffusion to increase the conversion of phenyl acetate and yield of diphenyl carbonate. Moreover, the coordination between titanium and ZIF-8 also endowed the catalysts with reasonable reusability.
机译:含有Tetra配位钛的催化剂已广泛用于酯交换。这些催化剂的设计中的关键问题是Tetra-协调钛的稳定性。在该研究中,通过使用十六烷基胺(HDA)表面活性剂作为结构引导剂,开发涂覆在沸石咪唑酯骨架(ZIF-8)上的中孔非晶钛氧化物。无定形TiO2壳的中孔表面区域可以简单地通过改变合成过程中HDA的剂量来控制。首次引入新的,高效和可回收的非均相催化剂以合成来自碳酸二甲酯和乙酸乙酸苯酯的二苯基碳酸酯。催化剂结构的特征在于X射线衍射,扫描电子显微镜,透射电子显微镜,氮吸附 - 解吸,傅里叶变换红外光谱和热重分析。还确定了Ti至Zn,HDA量,催化剂量,反应时间和可重用性对酯交换产物的产量的影响的影响。结果表明,TiO2壳促进的反应物和生产的中孔扩散,以增加苯基乙酸苯酯的转化和二苯基碳酸酯的产率。此外,钛和ZIF-8之间的配位也具有合理的可重用性赋予催化剂。

著录项

  • 来源
    《Journal of Materials Science》 |2019年第13期|共12页
  • 作者单位

    Chinese Acad Sci Chengdu Inst Organ Chem Chengdu 610041 Sichuan Peoples R China;

    Chongqing Univ Technol Sch Chem Engn Chongqing 400054 Peoples R China;

    Chinese Acad Sci Chengdu Inst Organ Chem Chengdu 610041 Sichuan Peoples R China;

    Chinese Acad Sci Chengdu Inst Organ Chem Chengdu 610041 Sichuan Peoples R China;

  • 收录信息
  • 原文格式 PDF
  • 正文语种 eng
  • 中图分类 工程材料学;
  • 关键词

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号