Laser clad specimens were fabricated to characterize the axial fatigue failure behavior of laser clad 4340 steel in the as-clad condition and for specifically designed clad specimens with pre-clad machining and post-clad surface grinding processes. Three types of laser clad fatigue test specimens (Type I, II and III) were tested to study fatigue failure behavior and were compared to the unclad 4340 steel substrate specimen. Type I specimen investigates fatigue failure behavior from the clad toe region of as-clad specimens. Type II specimen evaluates fatigue strength enhancement effects by pre-clad machining of a groove for depositing a clad layer with post-clad surface grinding to process the added clad layer in the groove to be flush with the substrate material. Type III specimen studies clad specimens with extended clad area and surface grinding to promote fatigue failure within the clad region. The fatigue S-N curve for Type 1,11 and III clad specimens were compared to the S-N curve for the substrate specimens to show the reduction in fatigue strength for as-clad Type I specimens, and machining methods to improve fatigue strength for Type II and Type III specimens. The fatigue strength of all laser-clad specimens was observed to be lower as compared to that of the unclad substrate specimen. (C) 2016Elsevier B.V. All rights reserved.
机译:制造激光包层标本,以表征激光包覆4340钢的轴向疲劳失效行为在作为包层的条件下,并专门设计的具有预包层加工和覆层后表面研磨方法的覆层标本。测试三种类型的激光包覆疲劳试验标本(I型,II和III)以研究疲劳失效行为,并与Unclad 4340钢基板标本进行比较。 I型样本研究了来自覆层标本的包层趾区域的疲劳失效行为。 II型试样通过预包覆的凹槽加工来评估疲劳强度增强效果,用于将包层层沉积与覆盖后的表面研磨以处理槽中的添加的包层与基板材料齐平。 III型试样研究包层标本,具有延长的包层区域和表面研磨,以促进包层内的疲劳失效。将1,11和III型包层标本的疲劳Sn曲线与底物标本的Sn曲线进行比较,以表明疲劳强度的疲劳强度降低,以及改善II型和型疲劳强度的加工方法III标本。与未甲壳底物标本相比,观察到所有激光包层标本的疲劳强度较低。 (c)2016LSEVIER B.V.保留所有权利。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号