Salt-Induced, Continuous Deposition of Supramolecular Iron(III)-Tannic Acid Complex

机译:盐致盐,连续沉积超分子铁(III) - 醛酸复合物

获取原文
获取原文并翻译 | 示例
           

摘要

One-step assembly of iron(III)-tannic acid (Fe3+-TA) complex forms nanothin (similar to 10 nm) films on various substrates within minutes. In this deposition scheme, however, the film does not grow continuously over time even though Fe3+-TA complex is still abundant in the coating solution. In this paper, we report that the salt addition dramatically changes the one-off coating characteristic to continuous one, and each salt has its optimum concentration (C-MFT) that produces maximum film thickness. For detailed investigation of the salt effects, we employed various salts, including LiCl, NaCl, KCl, CaCl2, SrCl2, BaCl2, NaBr, and NaNO3, and found that only cations played an important role in the continuous deposition of the Fe3+-TA complex, with smaller C-MFT values for the cations of higher valency and larger size. On the basis of the results, we suggested that the positively charged cations screened the negative surface charges of Fe3+-TA complex particles, leading to coagulation and continuous deposition, further supported by the zeta-potential measurement and time-resolved dynamic light-scattering analysis.
机译:铁(III) - 亚胺酸(Fe3 + -TA)复合物的一步组装在分钟内在各种底物上形成纳米素(类似于10nm)膜。然而,在该沉积方案中,即使Fe3 + -TA复合物在涂料溶液中仍然丰富,薄膜也不会随着时间的推移而不断增长。在本文中,我们报告说盐添加显着改变连续的一次性涂层特性,并且每种盐具有其最大浓度(C-MFT),其产生最大膜厚度。有关盐效应的详细研究,我们使用各种盐,包括LiCl,NaCl,KCl,CaCl2,SrCl2,Bacl2,NaBr和NaNO 3,并发现只有阳离子在Fe3 + -TA复合物的连续沉积中发挥着重要作用,对于更高的阳离子和更大尺寸的阳离子,具有较小的C-MFT值。在结果的基础上,我们建议带正电荷的阳离子筛选Fe3 + -TA复合颗粒的负面表面电荷,导致凝血和连续沉积,进一步支持Zeta-潜在的测量和时间分辨的动态光散射分析。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号