Boronate affinity materials, as effective sample enrichment sorbents for glycoproteomic analysis, have attracted increasing attention in recent years. However, most of boronate affinity materials suffer from an apparent limitation, limited binding strength. As a result, extraction of glycoproteins of trace concentration is rather difficult or impossible. In this study, we present a high boronate avidity monolithic capillary. Branched polyethyleneimine (PEI) was used as a scaffold to amplify the number of boronic acid moieties. While 2,4-difluoro-3-formyl-phenylboronic acid (DFFPBA), which exhibited ultrahigh affinity toward cis-diol-containing compounds, was employed as an affinity ligand. Due to the PEI-assisted synergistic multivalent binding, the monolithic column exhibited high boronate avidity toward glycoproteins, with binding constants of 10(-6)-10(-7) M. Such binding strength was the highest among already reported boronic acid-functionalized materials that can be used for glycoproteomic analysis. Besides, the boronate avidity monolithic column exhibited one additional beneficial feature, lowered binding (>= 6.5). These features greatly favored the selective enrichment of trace glycoproteins from real samples. The feasibility for practical applications was demonstrated with the selective enrichment of trace glycoproteins in human saliva. As compared with other boronate avidity/affinity materials, the boronate avidity monolithic capillary exhibited the best performance. (C) 2015 Elsevier B.V. All rights reserved.
机译:硼酸盐亲和材料作为糖蛋白组学分析的有效样品富集吸附剂,近年来受到越来越多的关注。然而,大多数硼酸酯亲和材料具有明显的局限性,有限的结合强度。结果,很难或不可能提取痕量浓度的糖蛋白。在这项研究中,我们提出了一种高硼酸亲和力整体毛细管。支链聚乙烯亚胺(PEI)用作支架以扩增硼酸部分的数量。对亲和性配体采用对含顺式二醇具有超高亲和性的2,4-二氟-3-甲酰基-苯基硼酸(DFFPBA)。由于PEI辅助的协同多价结合,整体柱对糖蛋白表现出高硼酸亲和力,结合常数为10(-6)-10(-7)M。在已报道的硼酸官能化反应中,这种结合强度最高可用于糖蛋白组学分析的材料。此外,硼酸盐亲和力整体柱还显示出另一项有益的功能,即降低了结合力(> = 6.5)。这些特征极大地促进了从真实样品中选择性富集微量糖蛋白。在人唾液中选择性富集微量糖蛋白证明了实际应用的可行性。与其他硼酸酯亲和力/亲和力材料相比,硼酸酯亲和力整体毛细管表现出最佳性能。 (C)2015 Elsevier B.V.保留所有权利。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号