The physical properties of microcapsules are largely influenced by the synthesis conditions such as weight ratio of core/shell material, agitation rate, reaction time, and different emulsifier. Different synthesis condition would lead to different property. It is an important issue for application in composites that require self-healing microcapsules possessing rough surface morphology, less adhesion, less core material permeability, appropriate diameter and core content, and adequate shell thickness. The properties of microcapsules influenced by the synthesis conditions were investigated systematically in this article. According to orthographic factorial design, the most influencing factor on microcapsule's yield, core material, average shell thickness and average diameter, are concluded, respectively. The synthesis parameters when the epoxy-containing microcapsules exhibit the optimum properties are concluded: 1.4: 1 for the weight ratio of core/shell material, 250 rpm for the agitation rate, 3 h for the reaction time and 1.5% content for the emulsifier DBS. The chemical structure of resultant microcapsules is confirmed by FT-IR, and core material of microcapsule exhibits reactivity through DSC measurement. Subsequently, the microcapsules are characterized by SEM, OM, and contact angle experiment so as to provide parameters of microcapsule's physical properties for making binary self-healing materials. As a result, the resultant microcapsules are suitable for fabricating self-healing materials.
机译:微胶囊的物理性质在很大程度上受合成条件的影响,例如核/壳材料的重量比,搅拌速率,反应时间和不同的乳化剂。不同的合成条件将导致不同的性质。对于在需要具有自修复微囊的复合材料中应用而言,这是一个重要问题,该微囊应具有粗糙的表面形态,更少的附着力,更少的芯材渗透性,合适的直径和芯含量以及足够的壳厚度。本文对合成条件对微胶囊性能的影响进行了系统的研究。根据正交法因子设计,得出了影响微胶囊产量,芯材,平均壳厚度和平均直径的最大影响因素。得出含环氧基微囊表现出最佳性能时的合成参数:核/壳材料的重量比为1.4:1,搅拌速率为250 rpm,反应时间为3 h,乳化剂DBS含量为1.5% 。通过FT-IR证实了所得微胶囊的化学结构,并且微胶囊的芯材通过DSC测量显示出反应性。随后,通过SEM,OM和接触角实验对微囊进行了表征,从而为制备二元自愈材料提供了微囊的物理性能参数。结果,所得的微囊适用于制造自修复材料。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号