摘要

Numerical predictions and experimental observations have been correlated to improve the qualitative understanding of the degree of thermal degradation occurring during the HVOF spray deposition of nylon-11. Particle residence time (similar to 1 ms) in the HVOF jet was insufficient for significant decomposition of the nylon-11, but was sufficient for noticeable discoloration (yellowing) of the particles of a powder with a mean particle size of 30 mu m. Experimental observation showed this to be the case even though numerical predictions indicated that the temperature of a 30 mu m diameter particle should be considerably higher than the upper degradation limit of nylon-11. Initial thermal oxidation of nylon-11 promotes the formation of carbon-carbon double bonds that strongly absorb in the visible spectrum even at concentrations of parts per million causing discoloration of the nylon. (c) 2007 Wiley Periodicals, Inc.
机译:数值预测和实验观察已被关联起来,以提高对尼龙11的HVOF喷涂过程中发生的热降解程度的定性理解。 HVOF射流中的颗粒停留时间(约1毫秒)不足以使尼龙11发生明显分解,但足以使平均粒径为30μm的粉末颗粒明显变色(泛黄)。实验观察表明情况确实如此,即使数值预测表明直径为30μm的颗粒的温度应明显高于尼龙11的降解上限。尼龙11的初始热氧化促进了碳-碳双键的形成,即使在百万分之几的浓度下,碳-碳双键也会在可见光谱中强烈吸收,从而导致尼龙变色。 (c)2007年Wiley Periodicals,Inc.

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号