Polyacrylonitrile (PAN) hollow fibers were pretreated with ammonium dibasic phosphate, then further oxidized in air, carbonized in nitrogen, and activated with carbon dioxide. The effects of oxidation time of PAN hollow fiber precursor on the microstructure, specific surface, pore size distribution, and adsorption properties of PAN-based activated carbon hollow fiber (PAN-ACHF) were studied in this work. Both of specific surface area and adsorption ratio to VB12 reach maximums when PAN hollow fibers are oxidized for 5 h in air. The adsorption ratios for creatinine are all higher than 90% over all oxidation time. After 5 h of oxidation, the number of pores on the surface obviously increases, and the pore size is uniform. After 7 h of oxidation, the number of macropores in PAN-ACHF increases. The dominant pore sizes of mesopores in PAN-ACHF range from 2 to 5 nm. (C) 2007 Wiley Periodicals, Inc.
机译:聚丙烯腈(PAN)中空纤维用磷酸氢二铵预处理,然后在空气中进一步氧化,在氮气中碳化,并用二氧化碳活化。本文研究了PAN中空纤维前体的氧化时间对PAN基活性炭中空纤维(PAN-ACHF)的微观结构,比表面积,孔径分布和吸附性能的影响。当PAN中空纤维在空气中氧化5小时时,比表面积和对VB12的吸附率均达到最大值。在所有氧化时间内,肌酸酐的吸附率均高于90%。氧化5 h后,表面孔的数量明显增加,且孔尺寸均匀。氧化7小时后,PAN-ACHF中的大孔数量增加。 PAN-ACHF中介孔的主要孔径为2至5 nm。 (C)2007 Wiley期刊公司

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号