Polyester nonwoven fabric samples were used to treat with aqueous solutions of water-soluble polyurethane (PU) containing the foaming agent, citric acid, or the mixtures of foaming agent and citric acid to examine the water remaining and the degradation of PU under the simulative condition of under ground. The results reveal that the viscosity of PU solutions could affect the values of pickup and add-on. The water remaining values for PU containing citric acid are higher than those for PU containing the foaming agent and PU containing the foaming agent and citric acid. The pore structures, nonwoven construction, and the pores caused by the aggregation of PU within/on the treated nonwoven fabrics can affect the water remaining. From the observation of SEM and the comparison of FTIR, the degradation of water-soluble PU resin is proved, which could form the rough porous surface of PU resin on the fiber surface as a factor improving the water remaining. The value of water remaining for PU containing citric after 60 weeks' treatment is significantly higher than the pristine nonwoven fabric (control). (c) 2006 Wiley Periodicals, Inc.
机译:聚酯无纺布样品用于处理含有发泡剂,柠檬酸或发泡剂与柠檬酸的混合物的水溶性聚氨酯(PU)水溶液,以在模拟条件下检查残留的水和PU的降解情况地下。结果表明,PU溶液的粘度可能会影响拾取值和添加值。包含柠檬酸的PU的水残留值高于包含发泡剂的PU和包含发泡剂和柠檬酸的PU的水残留值。孔隙结构,非织造结构以及在处理后的非织造织物中/上的PU聚集所引起的孔隙会影响残留的水分。从SEM的观察和FTIR的比较,证明了水溶性PU树脂的降解,其可以在纤维表面上形成PU树脂的粗糙多孔表面,作为改善残留水的因素。处理60周后,含有柠檬酸的PU的残留水值明显高于原始无纺布(对照)。 (c)2006年Wiley Periodicals,Inc.

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号