A new preparation method for polymer inclusion membrane (PIM) was developed. The preparation method-called post-treatment method-is very convenient to prepare a hollow fiber PIM. Using this method, a commercial cellulose triacetate (CTA) hollow fiber membrane can be easily converted into a hollow fiber PIM. Thus, a CTA hollow fiber membrane was allowed to swell in 2-nitrophenyln-octyl ether (NPOE) in the presence of chloroform as a solvent for CTA and N,N,M,M-tetraoctyl-3-oxapentane diamide (TODGA) as a carrier. After evaporating chloroform, a hollow fiber PEA containing NPOE and TODGA was obtained. The result of the transport experiment of cerium(III) ions using the hollow fiber PIM showed that cerium ions were effectively transported from the feed solution to the strip solution through the hollow fiber PIM, indicating that the hollow fiber PIM was successfully prepared using the post-treatment method. (c) 2006 Wiley Periodicals, Inc.
机译:开发了一种新的高分子包合物膜制备方法。称为后处理方法的制备方法对于制备中空纤维PIM非常方便。使用该方法,可以容易地将市售三乙酸纤维素(CTA)中空纤维膜转换成中空纤维PIM。因此,在氯仿存在下,将CTA中空纤维膜在2-硝基苯基-辛基醚(NPOE)中溶胀,作为CTA的溶剂,N,N,M,M-四辛基-3-氧杂戊烷二酰胺(TODGA)作为溶剂。载体。蒸发氯仿后,获得含有NPOE和TODGA的中空纤维PEA。使用中空纤维PIM传输铈(III)离子的实验结果表明,铈离子通过中空纤维PIM有效地从进料溶液传输到带状溶液,这表明中空纤维PIM是使用柱子成功制备的处理方法。 (c)2006年Wiley Periodicals,Inc.

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号