To improve equilibrium water content, dehydrothermally crosslinked poly(vinyl alcohol) (PVA) hydrogel was grafted with N-vinyl pyrrolidone (NVP) or acrylic acid (AA) monomer using gamma-radiation. Swelling behavior of the grafted hydrogels was studied in phosphate-buffered saline, and cell viability was evaluated using fibroblast cells from mouse connective tissue. Equilibrium water content of AA- and NVP-grafted PVA hydrogel ranged between 40-60% and 60-80%, respectively, depending on radiation dose and monomer concentration. For maximum degree of swelling, the optimum monomer concentration and radiation dose were 20% by weight and 20 kGy, respectively. Fibroblast cells seeded on NVP-grafted hydrogel had an extended oval morphology while those seeded on AA-grafted PVA had a rounded spherical morphology. These results support the use of NVP for grafting PVA to increase swelling and improve cell viability. (C) 2004 Wiley Periodicals, Inc. [References: 27]
机译:为了提高平衡水含量,使用γ-射线将脱氢热交联的聚乙烯醇(PVA)水凝胶与N-乙烯基吡咯烷酮(NVP)或丙烯酸(AA)单体接枝。在磷酸盐缓冲液中研究了接枝水凝胶的溶胀行为,并使用了来自小鼠结缔组织的成纤维细胞来评估细胞活力。 AA和NVP接枝的PVA水凝胶的平衡水含量分别在40-60%和60-80%之间,具体取决于辐射剂量和单体浓度。对于最大溶胀度,最佳单体浓度和辐射剂量分别为20%重量和20 kGy。接种在NVP接枝的水凝胶上的成纤维细胞具有扩展的椭圆形形态,而接种在AA接枝的PVA上的成纤维细胞具有圆形的球形形态。这些结果支持使用NVP移植PVA以增加肿胀并改善细胞活力。 (C)2004 Wiley Periodicals,Inc. [参考:27]

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号