It is well known that active screen plasma nitriding (ASPN) is driven using a pulsed D.C. power supply, due to several advantages such as improved control over temperature, nitrided layer phase composition and active species generation. In addition, the pulsed power supply helps to avoid the transition to the arc regime. The ASPN configuration in particular is preferred over conventional plasma nitriding due to complete elimination of edge effect, as plasma is not in direct contact with the samples. In this work, the influence of pulsed power supply parameters such as duty cycle, peak voltage, peak current and time averaged current is studied in an ASPN setup, on nitrided layer phase composition and surface hardness of austenitic stainless steel (ASS). In addition, optical emission spectroscopy (OES) is used to measure the excitation, vibrational and rotational temperatures (T-exc, T-vib, T-rot), nitrogen dissociation fraction and concentration of active species N-2(C-3 Pi(u)) and N-2(+)(B-2 Sigma(+)(u)) (in terms of emission intensities) to clarify the results obtained from surface characterization. The results show that keeping time-averaged current constant, the surface hardness decreases with the duty cycle of the pulsed D.C. power supply. The results from OES and surface analysis are correlated, and as a result plasma parameters (T-exc, T-vib, T-rot) and active species concentration (N, N-2, N-2(+)) are found to be important precursors in surface hardening of ASS. (C) 2016 Elsevier B.V. All rights reserved.
机译:众所周知,由于有几个优点,例如对温度的改进控制,氮化层相组成和活性物质的产生,使用脉冲直流电源来驱动有源屏等离子体氮化(ASPN)。另外,脉冲电源有助于避免过渡到电弧状态。由于完全消除了边缘效应,特别是ASPN配置优于常规等离子体氮化,因为等离子体不直接与样品接触。在这项工作中,在ASPN设置中研究了脉冲电源参数(例如占空比,峰值电压,峰值电流和时间平均电流)对奥氏体不锈钢(ASS)的氮化层相组成和表面硬度的影响。此外,使用光发射光谱法(OES)测量激发,振动和旋转温度(T-exc,T-vib,T-rot),氮解离分数和活性物质N-2(C-3 Pi的浓度) (u))和N-2(+)(B-2 Sigma(+)(u))(就发射强度而言)以阐明从表面表征获得的结果。结果表明,保持时间平均电流恒定,表面硬度随脉冲直流电源的占空比而降低。 OES和表面分析的结果相互关联,结果发现血浆参数(T-exc,T-vib,T-rot)和活性物质浓度(N,N-2,N-2(+))是ASS表面硬化的重要前体。 (C)2016 Elsevier B.V.保留所有权利。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号