Alkali-silica reaction (ASR)-performance testing: Influence of specimen pre-treatment, exposure conditions and prism size on alkali leaching and prism expansion

机译:碱二氧化硅反应(ASR)性能测试:样品预处理,暴露条件和棱镜尺寸对碱浸和棱镜膨胀的影响

获取原文
获取原文并翻译 | 示例
           

摘要

Whether or not concrete prism tests developed for assessment of alkali-silica reactivity of aggregates might be suitable for general ASR performance testing of concrete has been evaluated. This paper discusses how variations in specimen pre-treatment, ASR exposure conditions and prism size influence the rate and amount of alkali leaching and prism expansion, together with a discussion of consequences for ASR test procedures. Furthermore, results from some complementary tests are included.Generally, a remarkably high proportion of the in-mixed alkalis were leached out of the concrete prisms during the ASR exposure. For prisms exposed to 60 °C, the rate and amount of alkali leaching is the main controlling factor for the prism expansion. For less permeable concretes exposed to 38 °C, lack of internal moisture and lower rate of diffusion contributes to reduce the rate and extent of ASR expansion (reported in a separate paper).
机译:已经评估了开发用于评估骨料的碱-硅反应性的混凝土棱镜试验是否适合于混凝土的一般ASR性能测试。本文讨论了样品预处理,ASR暴露条件和棱镜尺寸的变化如何影响碱浸出和棱镜膨胀的速率和数量,并讨论了ASR测试程序的后果。此外,还包括一些补充试验的结果。通常,在ASR暴露期间,有很大比例的混合碱从混凝土棱柱中浸出。对于暴露于60°C的棱镜,碱浸的速度和量是棱镜膨胀的主要控制因素。对于暴露于38°C的渗透性较低的混凝土,内部水分的缺乏和较低的扩散速率有助于降低ASR膨胀的速率和程度(在另一篇论文中报道)。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号