Water-cooled slag (WS) and air-cooled slag (AS) with similar chemical compositions and produced from the same blast furnace were investigated for their hydraulic activities at different temperatures. The kinetics of hydration of WS-lime and AS-lime pastes were investigated at room temperature, 100 deg C, and 180 deg C by the determination of unreacted lime and combined water. The hydration products were identified by XRD. The variations in mechanical properties were correlated with the reaction kinetics and the typews of the hydration products. The change in the mechanism of slag hydration was also predicted. The AS studied exhibited significant reactivity at room temperature. Increasing the temperature to 100 deg C has no significant effect on the reactivity of either type of slag except during early hydration. However, the reactivity of AS increased much more than WS with hydrothermal activation at 180 deg C. calcium silicate hydrate (CSH) and plazolite formed in AS mixes. CSH, plazolite, and #alpha#-C_2SH formed in WS mixes at 180 deg C.
机译:研究了由同一高炉生产的化学成分相似的水冷炉渣(WS)和风冷炉渣(AS)在不同温度下的水力活动。通过测定未反应的石灰和混合水,在室温,100摄氏度和180摄氏度下研究了WS-石灰和AS-石灰浆料的水合动力学。通过XRD鉴定水合产物。力学性能的变化与反应动力学和水合产物的类型相关。还预测了渣水合机理的变化。所研究的AS在室温下表现出显着的反应性。将温度升高到100摄氏度对任何一种炉渣的反应性都没有显着影响,除了在早期水合期间。但是,在180℃水合硅酸钙水合物(CSH)和在AS混合物中形成的吡唑石中,AS的反应性比WS增长得多。在WS中形成的CSH,吡唑岩和#alpha#-C_2SH在180摄氏度下混合。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号