首页> 外文期刊>Colloid and polymer science >Synthesis and micellar characterization of thermosensitive amphiphilic poly(ε-caprolactone)-b-poly(N-vinylcaprolactam) block copolymers
【24h】

Synthesis and micellar characterization of thermosensitive amphiphilic poly(ε-caprolactone)-b-poly(N-vinylcaprolactam) block copolymers

机译:热敏两亲性聚(ε-己内酯)-b-聚(N-乙烯基己内酰胺)嵌段共聚物的合成和胶束表征

获取原文
获取原文并翻译 | 示例

摘要

Abstract Poly(ε-caprolactone)-b-poly(N-vinylcaprolac-tam) (PCL-b-PVCL) block copolymers were synthesized as new biocompatible, thermosensitive, amphiphilic block polymers by a combination of ring-opening polymerization and reversible addition-fragmentation chain transfer (RAFT) polymerization, and their thermosensitive micellar behavior was examined. The PCL macro-chain-transfer agent was first synthesized by converting the end group of PCL-OH to O-ethyl xanthate, which was subsequently used for the RAFT polymerization of iV-vinylcaprolactam. The critical micelle concentration of PCL-6-PVCL (M_(n,NMR)=56,300 g/mol, polydispersity index=1.18) was 0.026 mg/mL. The mean diameter of the PCL-Zj-PVCL micelles determined by transmission electron microscopy was 55 ±25 nm. The PCL-b-PVCL micelles exhibited repetitive aggregation and dispersion during reversible cooling and heating cycles between 20 and 40 °C due to the thermosensitive behavior of the PVCL shell. Overall, the PCL-b-PVCL block copolymers have potential applications in thermosensitive drug delivery applications.
机译:摘要结合开环聚合和可逆加成反应,合成了聚(ε-己内酯)-b-聚(N-乙烯基己内酰胺-tam)(PCL-b-PVCL)嵌段共聚物,作为新型的生物相容性,热敏性,两亲性嵌段聚合物。断裂链转移(RAFT)聚合,及其热敏胶束行为进行了检查。首先通过将PCL-OH的端基转化为O-乙基黄药,来合成PCL大链转移剂,然后将其用于iV-乙烯基己内酰胺的RAFT聚合。 PCL-6-PVCL的临界胶束浓度(M_(n,NMR)= 56,300 g / mol,多分散指数= 1.18)为0.026 mg / mL。通过透射电子显微镜测定的PCL-Zj-PVCL胶束的平均直径为55±25nm。由于PVCL壳的热敏特性,在20至40°C的可逆冷却和加热循环过程中,PCL-b-PVCL胶束表现出重复的聚集和分散。总体而言,PCL-b-PVCL嵌段共聚物在热敏药物递送应用中具有潜在的应用。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号