Effect of testing temperature from cryogenic to high temperatures on dynamic fracture properties in 5083 aluminum alloy

机译:低温至高温测试温度对5083铝合金动态断裂性能的影响

获取原文
获取原文并翻译 | 示例
           

摘要

Effect of temperature on mechanical properties of an 5083 aluminum alloy has been investigated for various testing temperatures from 10 to 773 K. For that purpose, the static tensile, dynamic fracture toughness test and fractography are carried out, and stop block method is employed to characterize fracture behavior at cryogenic temperatures. Mechanical properties such as 0.2percent proof stress and ultimate tensile strength increase with decreasing temperature. The high temperature embrittlement, which has been often reported for 5000 series alloys having high Mg content, was not observed in the present study. The dynamic fracture toughness value, J_d, and dynamic crack extension toughness, T_(mat), at 20 K are approximately 57percent and 74percent lower than that at 150 K, respectively. Fracture toughness at cryogenic temperatures shows strong dependence on formation of delamination cracks. The delamination cracks are initiated at grain boundaries. According to a SEM-EDX analysis, Mg is detected adjacent to the delamination cracks. Therefore, it is concluded that the formation of delamination cracks are concerned with #beta#(Al_3Mg_2) phase at the grain boundaries.
机译:在10至773 K的各种测试温度下,研究了温度对5083铝合金力学性能的影响。为此,进行了静态拉伸,动态断裂韧性测试和分形学分析,并采用阻块法进行了表征。低温下的断裂行为。诸如0.2%的极限应力和极限抗拉强度之类的机械性能会随着温度的降低而增加。在本研究中未观察到高温脆化,该脆化常被报告用于5000镁含量高的系列合金。动态断裂韧性值J_d和动态裂纹扩展韧性T_(mat)在20 K时分别比在150 K下低57%和74%。低温下的断裂韧性显示出对分层裂纹形成的强烈依赖性。分层裂纹始于晶界。根据SEM-EDX分析,在分层裂纹附近检测到Mg。因此,可以得出结论,分层裂纹的形成与晶界处的#beta#(Al_3Mg_2)相有关。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号