The effects of cooling rate and addition of Sr and Ti-B on microstructural features such as grain size, dendrite arm spacing, morphologies of eutectic silicon and iron rich compound were investigated for the Al-6.55 % Si-2.78 % Cu-0.59 % Fe-0.38 % Mg-0.34 % Mn alloy (JIS AC4B) . This alloy solidifies in the order of primaryα (Al) , α+α-AlFeMnSi eutectic, α+ Si eutectic, α+β-AlFeMnSi eutectic, α+ Si + Mg{sub}2Si eutectic andα+ Si + Al{sub}2Cu eutectic. The grain size, dendrite arm spacing,size of eutectic silicon particles and length of needle-like iron rich compound decrease as the cooling rate increases, and they are in linear relation on the logarithmic scale. The addition of a small amount of Ti-B markedly refines the grain size whilepractically unaffects the other solidification structures. At the cooling rates of 2.7 K/s, 14.4 K/s and 108.1 K/s, the eutectic silicon crystals fully modify with the addition of Sr more than 60 ppm, 13 ppm and 5 ppm respectively. The addition of Sr anda higher cooling rate tends to increase the formation of Chinese script type iron rich compound.
机译:研究了Al-6.55%Si-2.78%Cu-0.59%Fe的冷却速度以及Sr和Ti-B的添加对晶粒尺寸,枝晶臂间距,共晶硅和富铁化合物的微观结构特征的影响。 -0.38%Mg-0.34%Mn合金(JIS AC4B)。该合金按以下顺序凝固:初生α(Al),α+α-AlFeMnSi共晶,α+ Si共晶,α+β-AlFeMnSi共晶,α+ Si + Mg {sub} 2Si共晶和α+ Si + Al {sub} 2Cu共晶共晶的。晶粒尺寸,枝晶臂间距,共晶硅颗粒尺寸和针状富铁化合物的长度随着冷却速率的增加而减小,并且它们在对数尺度上呈线性关系。少量的Ti-B的加入可显着细化晶粒尺寸,而实际上不影响其他凝固组织。在2.7 K / s,14.4 K / s和108.1 K / s的冷却速率下,共晶硅晶体通过分别添加超过60 ppm,13 ppm和5 ppm的Sr充分改性。 Sr的添加和较高的冷却速率往往会增加汉字型富铁化合物的形成。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号