The combinations of the same stainless steels (SUS316L/SUS316L, SUS430L/SUS430L) and the different stainless steels (SUS316L/SUS430L) were joined with the pastes containing the stainless steel powder in MIM process. For joining the same stainless steels, the values of joined strength were 400 MPa for SUS316L/SUS316L compact sintered at 1623K, and 320 MPa for SUS430L/SUS430L compact sintered at 1373K respectively. For joining the different stainless steels, the values of joined strength for SUS316L/SUS430L compacts sintered at 1623 K were 330 MPa by using the paste with SUS316L, and 370 MPa by using the paste with SUS430L. At the joined area of SUS316L/SUS430L sintered compacts, the mixed layer (over 100 mum thickness) of ferrite and martensite phases was observed.
机译:在MIM工艺中,将相同的不锈钢(SUS316L / SUS316L,SUS430L / SUS430L)和不同的不锈钢(SUS316L / SUS430L)的组合与包含不锈钢粉末的糊剂结合在一起。为了接合相同的不锈钢,在1623K下烧结的SUS316L / SUS316L压块的接合强度值为400 MPa,在1373K下烧结的SUS430L / SUS430L压块的接合强度值为320 MPa。为了接合不同的不锈钢,在1623 K下烧结的SUS316L / SUS430L压块的接合强度值为使用SUS316L的糊剂为330 MPa,通过使用SUS430L的糊剂为370 MPa。在SUS316L / SUS430L烧结体的结合区域,观察到铁素体和马氏体相的混合层(厚度超过100微米)。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号