Submicrometre-sized LaPO4:Tb phosphor particles with a spherical shape and filled morphology were prepared by spray pyrolysis from a polymeric precursor solution containing citric acid and ethylene glycol. The LaPO4:Tb phosphor particles obtained from the aqueous spray solution had a hollow morphology and large size because of the high drying and decomposition rates of droplets. The mean sizes of the particles obtained from the aqueous spray and polymeric precursor solutions were each 1 and 0.8 mum, respectively. The optimum post-treatment temperature for the preparation of LaPO4:Tb phosphor particles with a spherical shape and high brightness was 1100 °C. The prepared LaPO4:Tb phosphor particles had high photoluminescence intensities under vacuum ultraviolet illumination of 147 nm.
机译:通过喷雾热解从含有柠檬酸和乙二醇的聚合物前体溶液中制备具有球形和填充形态的亚微米级LaPO4:Tb磷光体颗粒。由喷雾水溶液获得的LaPO 4:Tb磷光体颗粒由于液滴的高干燥和分解速率而具有中空形态和大尺寸。从水性喷雾溶液和聚合物前体溶液获得的颗粒的平均尺寸分​​别为1和0.8μm。制备球形高亮度LaPO4:Tb荧光粉的最佳后处理温度为1100°C。制备的LaPO 4:Tb荧光粉颗粒在147nm的真空紫外线照射下具有高的光致发光强度。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号