摘要

The specific peel system low-density polyethylene/isotactic polybutene-1 (PE-LD/iPB-1), which is often used for protective packages, was investigated in this study. The required peel force to open the package depends on the content of iPB-1 and on the processing conditions of the blowing process. Commercial products have a constant amount of iPB-1. Thus, a defined peel force can be adjusted by varying the processing conditions. The standard peel system PE-LD with 6 wt% iPB-1 was investigated in dependence on the processing conditions. The most important processing parameters of the processing line (extruder, die head, tube forming area) were varied and their influence on the peel properties was examined. For example the temperatures of the melt within the extruder, the size of the die gap within the die head, and the cooling behavior of the film bubble were investigated. Higher melt temperatures within the extruder decreased the peel force. The investigations also revealed a strong dependence of the peel force on the size of the die gap and on the degree of cooling. The new developed parameter time of solidification was used to characterize the cooling behavior.
机译:在这项研究中,研究了通常用于保护性包装的特殊剥离体系低密度聚乙烯/全同立构聚丁烯-1(PE-LD / iPB-1)。打开包装所需的剥离力取决于iPB-1的含量以及吹塑工艺的加工条件。商业产品具有恒定量的iPB-1。因此,可以通过改变加工条件来调节限定的剥离力。根据加工条件,对具有6 wt%iPB-1的标准剥离体系PE-LD进行了研究。改变生产线最重要的加工参数(挤出机,模头,管材形成面积),并检查其对剥离性能的影响。例如,研究了挤出机内熔体的温度,模头内模头间隙的大小以及薄膜气泡的冷却行为。挤出机内较高的熔体温度降低了剥离力。研究还表明,剥离力与模具间隙的大小和冷却程度有很大的关系。使用新开发的凝固时间参数来表征冷却行为。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号