Marginal and Internal Discrepancies Related to Margin Design of Ceramic Crowns Fabricated by a CAD/CAM System

机译:与CAD / CAM系统制作的陶瓷牙冠的边缘设计有关的边缘和内部差异

获取原文
获取原文并翻译 | 示例
   

获取外文期刊封面封底 >>

       

摘要

Purpose: The aim of this study was to evaluate the marginal discrepancy (MD) and internal discrepancy (ID) of ceramic crowns manufactured by a CAD/CAM system, having different finish lines. The hypotheses tested were that the finish line type would not influence the MD or ID of the crowns, and ID would not change in different regions. Materials and Methods: Three aluminum master dies (height: 5.5 mm, ?: 7.5 mm, conicity: 6°) with different finish lines (TC: tilted chamfer; LC: large chamfer; RS: rounded shoulder) were manufactured. Ten impressions were made from each master die using a modified parallelometer. Impressions were poured in type IV dental stone, and 30 ceramic crowns (IPS Empress CAD, Ivoclar) were subsequently milled. The crowns were fixed on their respective metallic die using a metallic fixation device. The distance between the external edges of the crown to the edge of the cervical preparation was performed at 50 points on the respective metallic die (MD analysis). With the replica technique, the ID values of each crown were further evaluated at 12 points equidistant to each other in three regions: radius (R), axial (A), and occlusal (Occl). The measurements were performed using an optical microscope (250×). The data (μm) were analyzed using ANOVA and Tukey′s test (5%). Results: The RS group (28.24 ± 11.42 μm) showed significantly lower MD values (p= 0.001) than those of TC (99.92 ± 18.32 μm) and LC (64.71 ± 25.64 μm) groups, both of which also differed statistically from one another. The ID results demonstrated significantly lower values in the LC group (183.01 ± 62.82 μm) (p= 0.0014) than those of TC (216.26 ± 83.23 μm) and RS (219.12 ± 87.24 μm) groups. ID results of TC and RS were not significantly different. Additionally, the ID results showed significant differences among the regions (p= 0.0001). The null hypotheses were rejected. Conclusion: The RS finish line produced MD values significantly lower than tilted and large chamfer, but large chamfer presented the lowest internal discrepancy values. Independent of the finish line type, internal discrepancy was the lowest in the axial region followed by radius and occlusal regions.
机译:目的:本研究的目的是评估由CAD / CAM系统制造的具有不同精加工线的陶瓷冠的边际差异(MD)和内部差异(ID)。检验的假设是终点线类型不会影响牙冠的MD或ID,并且ID在不同区域不会改变。材料和方法:制造了三个铝母模(高度:5.5毫米,Φ:7.5毫米,锥度:6°),具有不同的精加工线(TC:倾斜倒角; LC:大倒角; RS:圆肩)。使用改进的平行度仪从每个主模具中获得十个印模。将印模倒入IV型牙石中,然后研磨30个陶瓷冠(IPS Empress CAD,Ivoclar)。使用金属固定装置将冠固定在它们各自的金属模具上。在各个金属模具上的50个点进行牙冠的外边缘到子宫颈制剂边缘之间的距离(MD分析)。利用复制技术,进一步在三个区域(半径(R),轴向(A)和咬合(Occl))上等距的12个点处评估每个牙冠的ID值。使用光学显微镜(250×)进行测量。使用方差分析和Tukey检验(5%)分析数据(μm)。结果:RS组(28.24±11.42μm)的MD值(p = 0.001)显着低于TC(99.92±18.32μm)和LC(64.71±25.64μm)组,两者在统计学上也有差异。 ID结果表明,LC组(183.01±62.82μm)(p = 0.0014)的值明显低于TC(216.26±83.23μm)和RS(219.12±87.24μm)组的值。 TC和RS的ID结果没有显着差异。此外,ID结果显示区域之间存在显着差异(p = 0.0001)。零假设被拒绝了。结论:RS终点线产生的MD值明显低于倾斜的大倒角,但大倒角的内部差异值最低。与终点线类型无关,内部差异在轴向区域中最低,其次是半径和咬合区域。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号