Corrosion tests were performed in oxygen-saturated liquid Pb-Bi at 450degreesC and 550degreesC in a pot for 3000 h for Al-surface-treated steels containing various levels of Cr contents. The Al surface treatments were achieved using a gas diffusion method and a melt dipping method. Al2O3, FeAl2 and AlCr2 produced by the gas diffusion method exhibited corrosion resistance to liquid Pb-Bi, while the surface layer produced by the melt dipping method suffered a severe corrosion attack. Fe4Al13 and Fe2Al5 produced by the melt dipping method disappeared during the corrosion test at 550degreesC and only FeAl remained. (C) 2004 Elsevier B.V. All rights reserved.
机译:对于含不同含量Cr的经Al表面处理的钢,在锅中于450℃和550℃的氧饱和液态Pb-Bi中进行了3000小时的腐蚀试验。使用气体扩散法和熔融浸渍法进行Al表面处理。气体扩散法生产的Al2O3,FeAl2和AlCr2对液体Pb-Bi表现出耐蚀性,而熔浸法生产的表面层则受到严重的腐蚀。在550℃的腐蚀试验中,通过熔融浸渍法生成的Fe 4 Al 13和Fe 2 Al 5消失,仅残留FeAl。 (C)2004 Elsevier B.V.保留所有权利。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号