Heat resistant 12% Cr steels of the 16Cr12W2VTaB type (12Cr-2W-V-Ta-B-0.16C) provide a reduced activation material that can be used as a structural material for fusion and fast breeder reactors. The composition under study meets scientific and engineering requirements and has an optimal base element composition to provide a delta-ferrite content of no more than 2). It also has a minimum quantity of low melting impurity elements and non-metallic inclusions. Short-term tensile properties for the steel tested to 700 degreesC are provided after the standard heat treatment (normalization, temper). Rupture strength and creep properties for the steel depending on the initial heat treatment conditions are also given. The microstructural stability of the 16Cr12W2VTaB type steel at temperatures up to 650 degreesC is predicted to be good, and the properties of the steel after irradiation in BOR-60 are demonstrated. (C) 2002 Elsevier Science B.V. All rights reserved. [References: 8]
机译:16Cr12W2VTaB类型(12Cr-2W-V-Ta-B-0.16C)的耐热12%Cr钢提供了减少的活化材料,可以用作聚变反应堆和快速增殖反应堆的结构材料。所研究的成分符合科学和工程要求,并且具有最佳的基本元素成分,以提供不超过2%的铁素体含量。它还具有最少数量的低熔点杂质元素和非金属夹杂物。在标准热处理(正火,回火)之后,提供了经过700℃测试的钢材的短期拉伸性能。还给出了取决于初始热处理条件的钢的断裂强度和蠕变性能。预计16Cr12W2VTaB型钢在最高650℃的温度下具有良好的组织稳定性,并在BOR-60中辐照后证明了该钢的性能。 (C)2002 Elsevier Science B.V.保留所有权利。 [参考:8]

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号