The oxidation kinetics of boron carbide pellets were investigated in steam/argon mixtures in the temperature range 1200-1800 degrees C for steam partial pressures between 0.2 and 0.8 bar and total flows (steam + argon) between 2.5 and 10 g/min resulting in gas velocities from 1.01 to 5.34 m/s. A kinetic model for boron carbide pellet oxidation depending on temperature, steam partial pressure and flow velocity is obtained. The activation energy of the oxidation process was determined to be 163 +/- 8 kJ/mol. The strong influence of temperature and steam partial pressure on the boron carbide oxidation kinetics is confirmed. The obtained data suggest the coexistence of two kinetic regimes, one at 1200 degrees C and the other at 1400-1800 degrees C, with different dependence on steam partial pressure. (C) 2007 Elsevier B.V. All rights reserved.
机译:研究了碳化硼颗粒在1200-1800摄氏度温度范围内的蒸汽/氩气混合物中的氧化动力学,其中蒸汽分压在0.2至0.8 bar之间,总流量(蒸汽+氩气)在2.5至10 g / min之间,产生了气体速度从1.01到5.34 m / s。获得了取决于温度,蒸汽分压和流速的碳化硼粒料氧化的动力学模型。氧化过程的活化能被确定为163 +/- 8kJ / mol。证实了温度和蒸汽分压对碳化硼氧化动力学的强烈影响。获得的数据表明两种动力学机制共存,一种在1200摄氏度,另一种在1400-1800摄氏度,并且对蒸汽分压的依赖性不同。 (C)2007 Elsevier B.V.保留所有权利。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号