Objectives: The purpose of this clinical study was to describe outcome variables of all-ceramic and metal-ceramic implant-supported, single-tooth restorations. Materials and methods: A total of 59 patients (mean age: 27.9 years) with tooth agenesis and treated with 98 implant-supported single-tooth restorations were included in this study. Two patients did not attend baseline examination, but all patients were followed for 3 years. The implants supported 52 zirconia, 21 titanium and 25 gold alloy abutments, which retained 64 all-ceramic and 34 metal-ceramic crowns. At baseline and 3-year follow-up examinations, the biological outcome variables such as survival rate of implants, marginal bone level, modified Plaque Index (mPlI), modified Sulcus Bleeding Index (mBI) and biological complications were registered. The technical outcome variables included abutment and crown survival rate, marginal adaptation of crowns, cement excess and technical complications. The aesthetic outcome was assessed by using the Copenhagen Index Score, and the patient-reported outcomes were recorded using the OHIP-49 questionnaire. The statistical analyses were mainly performed by using mixed model of ANOVA for quantitative data and PROC NLMIXED for ordinal categorical data. Results: The 3-year survival rate was 100% for implants and 97% for abutments and crowns. Significantly more marginal bone loss was registered at gold-alloy compared to zirconia abutments (P = 0.040). The mPlI and mBI were not significantly different at three abutment materials. The frequency of biological complications was higher at restorations with all-ceramic restorations than metal-ceramic crowns. Loss of retention, which was only observed at metal-ceramic crowns, was the most frequent technical complication, and the marginal adaptations of all-ceramic crowns were significantly less optimal than metal-ceramic crowns (P = 0.020). The professional-reported aesthetic outcome demonstrated significantly superior colour match of all-ceramic over metal-ceramic crowns (P = 0.015). However, no significant differences in the other aesthetic parameters at various restoration materials were registered. After 3 years, the patient-reported outcome variables at different restoration materials were not significantly different. Conclusion: The biological outcomes at the zirconia and metal abutments were comparable. All-ceramic crowns demonstrated better colour match, but higher frequency of marginal discrepancy compared to metal-ceramic crowns. Generally, the patients noticed no difference in aesthetic outcome of all-ceramic and metal-ceramic restorations.
机译:目的:本临床研究的目的是描述全陶瓷和金属陶瓷植入物支持的单齿修复体的结果变量。材料和方法:本研究共纳入59例无牙发育不良的患者(平均年龄:27.9岁),并接受98种植入物支持的单齿修复体的治疗。两名患者未参加基线检查,但所有患者均已随访3年。植入物支持52个氧化锆,21个钛和25个金合金基台,这些基台保留了64个全陶瓷冠和34个金属陶瓷冠。在基线和3年的随访检查中,记录了生物学结果变量,例如植入物的存活率,边缘骨水平,改良的斑块指数(mPlI),改良的沟出血指数(mBI)和生物学并发症。技术结果变量包括基台和牙冠存活率,牙冠的边缘适应性,骨水泥过多和技术并发症。使用哥本哈根指数评分评估美学结果,并使用OHIP-49问卷记录患者报告的结果。统计分析主要通过使用ANOVA的混合模型进行定量数据,使用PROC NLMIXED进行序数分类数据进行。结果:植入物的3年生存率是100%,基台和牙冠的3年生存率是97%。与氧化锆基台相比,金合金的边缘骨损失显着增加(P = 0.040)。在三种基台材料上,mPlI和mBI没有显着差异。在全瓷修复体中,生物并发症的发生频率高于金属陶瓷冠。仅在金属陶瓷冠上观察到的保留力丧失是最常见的技术并发症,全陶瓷冠的边缘适应性明显不如金属陶瓷冠的最佳适应性(P = 0.020)。专业人士报告的美学结果表明,全瓷冠比金属陶瓷冠的配色显着优越(P = 0.015)。但是,在各种修复材料上,其他美学参数均无显着差异。 3年后,患者报告的不同修复材料的结果变量无显着差异。结论:氧化锆和金属基台的生物学结果相当。与金属陶瓷冠相比,全陶瓷冠显示出更好的色彩匹配,但边缘差异的频率更高。通常,患者注意到全瓷修复体和金属陶瓷修复体的美学效果没有差异。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号