A novel method for the fabrication of an intermediate temperature proton conducting composite membrane was developed. Cesium dihydrogen phosphate, CsH2PO4 (CDP), was electrospun to obtain a highly interconnected proton conducting fibre mat. CsH2PO4 was heat treated above its dehydration temperature (T_(dehy) ~ 230 °C) in order to induce a partial polymerisation. The partially polymerised material produced a viscous aqueous solution which could be electrospun in the absence of a carrier polymer, thus leading to pure inorganic fibres. The electrospun fibre mats were characterised in terms of composition, structure and morphology by XRD, MAS NMR and SEM and their proton conductivity determined by electrochemical impedance spectroscopy. The electrospun fibres (CDPf) showed a maximum proton conductivity of 8 x 10~(-3) S cm~(-1) at 250 °C.
机译:开发了一种制备中温质子传导复合膜的新方法。对磷酸二氢铯CsH2PO4(CDP)进行电纺以获得高度互连的质子传导纤维毡。为了使其发生部分聚合,对CsH2PO4进行了高于其脱水温度(T_(dehy)〜230°C)的热处理。部分聚合的材料产生了粘稠的水溶液,该溶液可以在不存在载体聚合物的情况下进行电纺丝,从而得到纯的无机纤维。通过XRD,MAS NMR和SEM对电纺纤维毡的组成,结构和形态进行了表征,并通过电化学阻抗谱确定了质子电导率。在250°C时,电纺纤维(CDPf)的最大质子传导率为8 x 10〜(-3)S cm〜(-1)。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号