首页> 外文期刊>Journal of Materials Processing Technology >Separation of PRMMC into matrix alloy and reinforcements by nozzle filtering method
【24h】

Separation of PRMMC into matrix alloy and reinforcements by nozzle filtering method

机译:通过喷嘴过滤法将PRMMC分离为基体合金和增强材料

获取原文
获取原文并翻译 | 示例
       

摘要

The SiC{sub}p/Al-4mass%Cu alloy composites fabricated by a low-pressure infiltration process (LPI process) were remelted and separated by nozzle filtering method. In the separation process, the PRMMC specimen was placed in a container with a small nozzle at the bottom. The molten PRMMC was forced to flow out through the nozzle by applying a certain pressure of Ar gas. Most of the molten matrix alloy flowed out through the nozzle and the remainder in the container consisted of SiC particles and a part of the matrix alloy. The particle volume fraction of the remainder was higher than that of the original PRMMC and the remainder would work as a filter to separate SiC particles from the matrix alloy melt. When nozzle tip angle was ranged from 60° to 120°, about 80% of matrix alloy in the PRMMC was separated and few SiC particles were observed in the separated matrix alloy. The surface of recovered SiC particles became slightly roughened due to the reaction with the molten matrix during the separation process. However, this is not expected to affect their reuse.
机译:通过低压浸渗法(LPI法)制备的SiC {sub} p / Al-4质量%Cu合金复合材料通过喷嘴过滤法重熔分离。在分离过程中,将PRMMC标本放置在底部带有小喷嘴的容器中。通过施加一定压力的Ar气体,迫使熔融的PRMMC通过喷嘴流出。大部分熔融基体合金通过喷嘴流出,容器中的其余部分由SiC颗粒和一部分基体合金组成。其余部分的颗粒体积分数高于原始PRMMC的颗粒体积分数,其余部分将用作将SiC颗粒与基体合金熔体分离的过滤器。当喷嘴尖端角在60°至120°范围内时,PRMMC中约80%的基体合金被分离,并且在分离的基体合金中观察到很少的SiC颗粒。由于在分离过程中与熔融基质的反应,回收的SiC颗粒的表面略微变粗糙。但是,这不会影响它们的重用。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号