OBJECTIVE: To evaluate the 6-year performance of two glass fiber-reinforced packable resin composites in Class II cavities. METHODS: Sixty-three participants received 87 medium to large, cervically dentin bordered, Class II restorations of two fiber-reinforced resin composites, 42 Nulite F (N) and 45 Alert (A). The restorations were evaluated clinically, according to slightly modified USPHS criteria at baseline, after 6 months, and yearly during 6 years. RESULTS: At 2 years the cumulative failure frequencies for N and A were 4.8% and 2.2%, respectively, which increased at 6 years to 25.0% and 12.8%. Reasons for failure were secondary caries, material and cusp fracture. The majority of the failures occurred after 3 years. Secondary caries occurred between 4 and 6 years. The incorporation of fibers resulted in very rough surface characteristics. CONCLUSIONS: A rather high failure rate was observed for one of the fiber-reinforced resin composites, while the other fulfilled the ADA criteria. The occurrenceof most failures after 3 years indicated the necessity of long-term evaluations of new materials.
机译:目的:评估两种玻璃纤维增​​强的可填充树脂复合材料在II型腔中的6年性能。方法:63名参与者接受了87种中型至大型,以宫颈牙本质为边界的II类修复物,其中两种纤维增强树脂复合材料分别为42 Nulite F(N)和45 Alert(A)。根据基线时,6个月后和6年中每年的USPHS标准稍作修改,对修复体进行临床评估。结果:在2年时,N和A的累积失效频率分别为4.8%和2.2%,在6年时增加到25.0%和12.8%。失败的原因是继发性龋齿,物质和尖瓣断裂。大多数故障发生在3年后。次生龋齿发生在4至6年之间。纤维的掺入导致非常粗糙的表面特性。结论:其中一种纤维增强树脂复合材料观察到相当高的失效率,而另一种满足ADA标准。 3年后大多数故障的发生表明有必要对新材料进行长期评估。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号