For the utilization of product from wood liquefaction by ionic liquid, the liquefied product was sulfonated by chlorosulfonic acid as a sulfonating agent, and the product of wood liquefaction sulfonation (WLS) was obtained. The characterization of WLS is determined using FTIR, and the strong absorption peak of sulfonic group is clear. The suitable reaction conditions are as follows, the mass ratio of chlorosulfonic acid to liquefied wood and formaldehyde to liquefied wood are 0.8:1 and 0.9:1, reaction temperature of sulfonation and condensation are at 85°C and 90°C, reaction time of sulfonation and condensation are for 2.5 and 3.0 hours. When the solution concentration of WLS is 15 g ·L~(-1), the surface tension is 46.9 mN·m~(-1). In the formula of seed coating agent, WLS shows better suspension property and less change of viscosity in impact test than that of conventional surfactants, also, it can generate synergy effects with the other surfactants to make higher suspending rate in binary or ternary mixed system than that in single system.
机译:为了利用通过离子液体的木材液化的产物,将液化的产物用氯磺酸作为磺化剂进行磺化,从而获得木材液化的磺化产物(WLS)。使用FTIR测定WLS的特征,并且磺酸基的强吸收峰清晰可见。合适的反应条件如下:氯磺酸与液化木材的质量比和甲醛与液化木材的质量比为0.8:1和0.9:1,磺化和缩合的反应温度为85°C和90°C,反应时间为磺化和缩合分别进行2.5和3.0小时。 WLS的溶液浓度为15g·L〜(-1)时,表面张力为46.9mN·m〜(-1)。在种子包衣剂配方中,WLS在冲击试验中显示出比常规表面活性剂更好的悬浮性和较小的粘度变化,并且与其他表面活性剂产生协同作用,从而使二元或三元混合体系中的悬浮速率更高。在单个系统中。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号