A new method is presented for the development of natural fiber composites of high-performance thermoplastic polymers considering poly(phenylene ether) (PPE) and wood flour as an example system. The large gap between the high processing temperature of PPE, typically between 280 and 320degreesC, and the low decomposition temperature of wood flour, about 200degreesC, was reduced by using a reactive solvent, a low molecular weight epoxy. The epoxy formed miscible blends with PPE, which offered much lower viscosity compared to PPE and processing temperatures well below the decomposition temperature of wood flour. In addition, the epoxy component accumulated around the polar wood flour particles upon polymerization during the fabrication step. The composite materials consisted of a thermoplastic continuous phase and two dispersed phases, one of polymerized epoxy and the other of wood flour particles coated with polymerized epoxy. These composites offered a significant reduction in density and better mechanical and physical properties when compared to commercially available grades of engineering polymer blends filled with short glass fibers. (C) 2002 Wiley Periodicals, Inc. [References: 37]
机译:以聚苯醚(PPE)和木粉为例,提出了一种开发高性能热塑性聚合物天然纤维复合材料的新方法。通过使用反应性溶剂(一种低分子量的环氧树脂),可以降低PPE的较高加工温度(通常在280至320摄氏度之间)与木粉的较低分解温度(约200摄氏度)之间的较大差距。环氧形成的与PPE的可混溶共混物,与PPE相比,其粘度低得多,加工温度远低于木粉的分解温度。另外,在制造步骤期间,聚合时在极性木粉颗粒周围积聚环氧组分。该复合材料由热塑性连续相和两个分散相组成,一种是聚合环氧树脂,另一种是涂有聚合环氧树脂的木粉颗粒。与填充短玻璃纤维的市售级工程聚合物混合物相比,这些复合材料可显着降低密度,并具有更好的机械和物理性能。 (C)2002 Wiley Periodicals,Inc. [参考:37]

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号