Extraction of manganese from manganese dioxide ores was investigated using corncob as a reducing agent in dilute sulfuric acid medium. The effects of corncob amount, concentration of sulfuric acid, leaching temperature, reaction time and ore particle size were discussed. The leaching efficiency of manganese reached 92.8percent while iron dissolved was 24.6percent under the optimal condition which was determined for 10 g of manganese dioxide ore as corncob amount of 3 g, ore size of 75 mum, sulfuric acid concentration of 1.9 mol/L, leaching temperature of 85 degC for 60 min. In a word, the method provided a good leaching yield while making a productive use of corncob.
机译:使用玉米芯作为还原剂在稀硫酸介质中研究了从二氧化锰矿石中提取锰的方法。讨论了玉米芯量,硫酸浓度,浸出温度,反应时间和矿石粒度的影响。在最佳条件下,锰的浸出率达到了92.8%,铁的溶出率为24.6%。在最佳条件下,以玉米芯为3 g,矿石大小为75 um,硫酸浓度为1.9 mol / L来测定10 g二氧化锰矿石。浸出温度为85摄氏度,持续60分钟。简而言之,该方法在有效利用玉米芯的同时提供了良好的浸出率。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号