首页> 外文期刊>Hydrometallurgy >Study in reduction-roast leaching manganese from low-grade manganese dioxide ores using cornstalk as reductant
【24h】

Study in reduction-roast leaching manganese from low-grade manganese dioxide ores using cornstalk as reductant

机译:以玉米秸秆为还原剂的低品位二氧化锰矿石还原焙烧浸出锰的研究

获取原文
获取原文并翻译 | 示例
       

摘要

In this study cornstalk was used as reductant for reduction roasting of low-grade manganese dioxide ores, and sulfuric acid was used as leaching solvent for the roasted ore. The effects of weight ratio of ore to cornstalk, roasting temperature, roasting time, ore particle size, leaching temperature, stirring speed and sulfuric acid concentration on the leaching recovery were discussed. The leaching recovery of manganese reached 90.2 percent under the optimal condition which was determined as manganese dioxide ore to cornstalk weight ratio of 10:3, roasting temperature of 500 deg C for 80 min, leaching stirring speed of 400 r/min, sulfuric acid concentration of 3 mol/L, leaching temperature of 50 deg C for 40 min.
机译:在本研究中,玉米秸秆用作还原剂,用于还原低品位的二氧化锰矿石,硫酸用作浸提溶剂。讨论了矿粉与玉米秸秆的重量比,焙烧温度,焙烧时间,矿石粒度,浸出温度,搅拌速度和硫酸浓度对浸出回收率的影响。在最佳条件下,锰的浸出回收率达到90.2%,该条件是二氧化锰与玉米秸秆的重量比为10:3,焙烧温度为500℃,焙烧时间为80分钟,浸出搅拌速度为400 r / min,硫酸浓度为3 mol / L,浸出温度50摄氏度,持续40分钟。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号