A photoreactor has been set up to study the photodegradation of volatile organic compound (VOC) in situ. In the reactor, TiO2 and Pt/TiO2 photocatalysts were immobilized on to UV-transparent quartz support Scanning electron microscope (SEM) studies and Brunauer-Emmett-Teller (BET) surface area measurements revealed that the quartz fiber support was mostly coated with catalyst with a total surface area of 4.0 +/- 0.3 m(2)/g. The photocatalytic activity of the photocatalysts was evaluated for the photodegradation of 160 ppm toluene-laden air. It was found that 50-70% of toluene was degraded within the first 5 min of UV illumination. Both TiO2 and Pt/TiO2 photocatalysts suffered from deactivation after 18 hours of continuous operation, and the photocatalysts' activity was significantly reduced. However, platinization doubled the photocatalyst life and delayed the onset of de-activation. The presence of moisture was found to shift the onset of catalyst de-activation to an earlier time. It is concluded that the de-activation of the photocatalyst was due to the accumulation of intermediates on the photocatalysts surface preventing the toluene being adsorbed on the photocatalyst surface for degradation.
机译:已经建立了光反应器来研究挥发性有机化合物(VOC)的光降解。在反应器中,TiO2和Pt / TiO2光催化剂被固定在紫外线透明的石英载体上。扫描电子显微镜(SEM)研究和Brunauer-Emmett-Teller(BET)表面积测量表明,石英纤维载体大部分被催化剂涂覆总表面积为4.0 +/- 0.3 m(2)/ g。对于160ppm的负载甲苯的空气的光降解性,评价了光催化剂的光催化活性。发现在紫外线照射的前5分钟内50-70%的甲苯被降解。连续运行18小时后,TiO2和Pt / TiO2光催化剂均失活,并且光催化剂的活性明显降低。但是,镀铂使光催化剂寿命延长了一倍,并延迟了失活的开始。发现水分的存在将催化剂失活的开始转移到更早的时间。结论是,光催化剂的失活是由于中间体在光催化剂表面上的积聚,从而阻止了甲苯被吸附在光催化剂表面上而降解。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号